Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 38.44 - 49.6 g/10 min @Load 5.00 kg, Temperature 345 °C |
38.44 - 49.6 g/10 min @Load 11.0 lb, Temperature 653 °F |
ASTM D1238 |
Gharda Chemicals Gafone S 1500 Polysulfone (PS)
(discontinued **) Characteristics: High Temperature Resistance - Tg 189°C Excellent Clarity Excellent Mechanical & Electrical properties Easy to process Very good Hydrolytic Resistance Applications: Elec.. |