Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Flexirene® CM 50 Butene Copolymer Linear Low Density Polyethylene Flexirene CM 50 is a butene copolymer with medium density (C4-LLDPE), with antioxidants, suitable for cast film extrusion.Main Applications: Flexirene CM 50 is a highly stiff product and it is reco.. |
|||
Melt Flow | 4.1 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.1 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers MS 150 IF Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Melt Flow | 4.1 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.1 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Network Polymers MS 160 Styrene Methyl Methacrylate Terpolymer Description: Styrene Methyl Methacrylate TerpolymerInformation provided by Network Polymers Inc. |
|||
Melt Flow | 4.1 g/10 min @Load 2.16 kg, Temperature 210 °C |
4.1 g/10 min @Load 4.76 lb, Temperature 410 °F |
|
Reliance Industries PVAXX H65 The key property of all PVAXX polymer is this product`s unique capacity to biodegrade into non-toxic residues under both aerobic and non-aerobic conditions.Information provided by Reliance Industrie.. |
|||
Melt Flow | 4.1 g/10 min | 4.1 g/10 min | Exxon Method |
ExxonMobil Escorene® LD-409 EVA for Low Voltage Insulation
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A crosslinkable, 9.9% vinyl acetate copolymer designed for electrical applications.Applications: Designed to be blended with a suitable masterbatch .. |
|||
Melt Flow | 4.1 - 7.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
4.1 - 7.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Iran Petrochemical (PCC) PC 0407 Polycarbonate Suitable for extrusion, injection, and blow moldingInformation provided by Iran Petrochemical Commercial Co. |
|||
Melt Flow | 4.1 - 8.0 g/10 min | 4.1 - 8.0 g/10 min | A |
Shandong Dongyue Shenzhou New Material Co DS600 Perfluorinated Ethylene-Propylene Copolymer Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene resin is the copolymer of the TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and.. |
|||
Melt Flow | 4.1 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.1 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Styrolution PS 542N HIPS Styrolution PS 542N is an impact polystyrene with high heat resistance.Information provided by Styrolution |
|||
Melt Flow | 4.1 g/10 min @Load 5.00 kg, Temperature 250 °C |
4.1 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D 1238 |
SABIC Innovative Plastics Xenoy® X5600WX PC+POLYESTER (Europe-Africa-Middle East) Unreinforced, opaque Polyester+PC alloy. Chemical resistance, dimensional stability and mechanical performance. UV Stabilized. Mold ReleaseThis data was supplied by SABIC-IP for the Europe-Africa-Mi.. |
|||
Melt Flow | 4.1 g/10 min | 4.1 g/10 min | ASTM D1238L |
Total PPH 3462 Polypropylene, Extrusion Grade Homopolymer extrusion grade for slit film and fibrillated tapesProcess Stability --FINA 3462 is formulated to give excellent process stability in extrusion applications.FDA - FINA 3462 complies with.. |
|||
Melt Flow | 4.1 g/10 min @Load 1.20 kg, Temperature 300 °C |
4.1 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® 3206 Polycarbonate ISO 7391-PC,M,(,,)-05-9MVR (300 °C/1.2 kg) 4.0 cm3/10 minFood contact qualityHigh viscosityGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CExtrusionAvailable in transpar.. |
|||
Melt Flow | 4.1 g/10 min @Load 5.00 kg, Temperature 250 °C |
4.1 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D 1238 |
SABIC Innovative Plastics Xenoy® X5600WX PC+POLYESTER (Asia Pacific) Unreinforced, opaque Polyester+PC alloy. Chemical resistance, dimensional stability and mechanical performance. UV Stabilized. Mold ReleaseThis data was supplied by SABIC-IP for the Asia Pacific reg.. |