Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Flexirene® CM 50 Butene Copolymer Linear Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Butene, Film
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Flexirene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Flexirene® CM 50 Butene Copolymer Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Flexirene CM 50 is a butene copolymer with medium density (C4-LLDPE), with antioxidants, suitable for cast film extrusion.Main Applications: Flexirene CM 50 is a highly stiff product and it is recommended for the production of coextruded stretch film in slip-cling formulations where it acts as the slip layer. Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.938 g/cc
0.938 g/cc
ISO 1183
Thickness 10.0 - 50.0 microns
0.394 - 1.97 mil
Recommended
Melt Flow 4.1 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.1 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 17.0 MPa
2470 psi
ISO 527-3
Film Tensile Strength at Yield, TD 16.0 MPa
2320 psi
ISO 527-3
Film Elongation at Break, MD 600 %
600 %
ISO 527-3
Film Elongation at Break, TD 700 %
700 %
ISO 527-3
Coefficient of Friction, Dynamic >= 0.50
>= 0.50
ISO 8295
Elmendorf Tear Strength, MD 0.8152 g/micron
20.71 g/mil
ISO 6383-2
Elmendorf Tear Strength, TD 2.038 g/micron
51.77 g/mil
ISO 6383-2
Dart Drop Test 45.0 g
0.0992 lb
F50; ISO 7765-1
Film Tensile Strength at Break, MD 25.0 MPa
3630 psi
ISO 527-3
Film Tensile Strength at Break, TD 20.0 MPa
2900 psi
ISO 527-3
1% Secant Modulus, MD 350 MPa
50800 psi
ISO 527-3
1% Secant Modulus, TD 370 MPa
53700 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 127 °C
261 °F
Internal method
Vicat Softening Point 118 °C

@Load 1.00 kg
244 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Optical Properties Metric English Comments
Haze 8.0 %
8.0 %
ISO 14782
Gloss 75 %
75 %
45°; ASTM D2457