Polymer Property : Melt Flow = 4.28 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 4.28 g/10 min

@Load 10.0 kg,
Temperature 220 °C
4.28 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Styrolution Luran® S 776 S Colored ASA
Description: Injection molding grade with good toughness and strength. Uses include parts for garden equipment, parts for office chairs and antennas.Information provided by STYROLUTION, which is a j..
Melt Flow 4.28 g/10 min

@Load 10.0 kg,
Temperature 220 °C
4.28 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Styrolution Luran® S 776 S UV ASA
Description: Injection molding grade with good toughness and strength. Uses include parts for garden equipment, parts for office chairs and antennas.Information provided by STYROLUTION, which is a j..