Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 42 g/10 min @Load 5.00 kg, Temperature 190 °C |
42 g/10 min @Load 11.0 lb, Temperature 374 °F |
Procedure A; ASTM D1238 |
PolyOne Elastamax™ HTE 3050 Polyvinyl Chloride + NBR (PVC+NBR) Elastamax™ HTE Series thermoplastic elastomers (TPEs) are based upon compounded blends of PVC resins and nitrile rubber. These elastomeric materials provide outstanding resistance to hydrocarbons a.. |
|||
Melt Flow | 42 g/10 min @Load 5.00 kg, Temperature 260 °C |
42 g/10 min @Load 11.0 lb, Temperature 500 °F |
Calculated from MVR using melt density; ISO 1133 |
Lanxess Pocan® T 7391 POS151 000000 PBT + PET, 45% Glass Fiber
(discontinued **) PBT+PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load, UV-stabilized |
|||
Melt Flow | 42 g/10 min | 42 g/10 min | ISO 1133 |
Solvay Engineered Polymers SEQUEL® 1405 TPO
(discontinued **) Description: SEQUEL® 1405 engineered polyolefin material is designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, high flow and e.. |
|||
Melt Flow | 42 g/10 min @Load 2.16 kg, Temperature 380 °C |
42 g/10 min @Load 4.76 lb, Temperature 716 °F |
ASTM D1238 |
Solvay Specialty Polymers Veradel® 3400 Polyethersulfone (PESU)
(Unverified Data**) Veradel 3400 polyethersulfone (PESU) is a high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boi.. |
|||
Melt Flow | 42 g/10 min @Load 2.16 kg, Temperature 190 °C |
42 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LyondellBasell Alathon® H5642 High Density Polyethylene, Injection Molding Grade
(discontinued **) ALATHON H5642 is a multi-purpose, narrow molecular weight distribution high-flow resin featuring enhanced processing and thermal stability for fast cycling. This resin exhibits good color and organo.. |
|||
Melt Flow | 42 g/10 min @Load 10.0 kg, Temperature 220 °C |
42 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical LI970HF Co-Extrusion ASA Description: Good Weatherability, Scratch Resistance, High FlowApplication: Window Profile, Siding, Rain GutterCAS: 26299-47-8Information provided by LG Chemical |
|||
Melt Flow | 42 g/10 min | 42 g/10 min | ASTM D1238 |
Kolon KOCETAL® K900 Standard Grade Acetal Resin Very low viscosity grade. Applications: Thin and large products.Information provided by API-Kolon. |
|||
Melt Flow | 42 g/10 min @Load 2.16 kg, Temperature 320 °C |
42 g/10 min @Load 4.76 lb, Temperature 608 °F |
ASTM D1238 |
Kuraray Genestarâ„¢ G1350H Nylon, 35% Glass Filled Standard HB grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm. It is suitable for use in .. |
|||
Melt Flow | 42 g/10 min @Load 5.00 kg, Temperature 290 °C |
42 g/10 min @Load 11.0 lb, Temperature 554 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Durethan® DP AKV 30 X HR EF 900116 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, hydrolysis and good heat-ageing resistance, good flowability (Easy Flow) |
|||
Melt Flow | 42 g/10 min @Load 2.16 kg, Temperature 260 °C |
42 g/10 min @Load 4.76 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Pocan® B 3225 XF 000000 PBT, 20% Glass Fiber PBT, 20% glass fibers, injection molding, improved flowability |
|||
Melt Flow | 42 g/10 min @Load 5.00 kg, Temperature 260 °C |
42 g/10 min @Load 11.0 lb, Temperature 500 °F |
Calculated from MVR using melt density; ISO 1133 |
Lanxess Pocan® T 7391 000000 PBT + PET, 45% Glass Fiber PBT+PET, 45% glass fibers, injection molding, improved surface finish, increased temperature peak load |
|||
Melt Flow | 42 g/10 min @Load 5.00 kg, Temperature 250 °C |
42 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 420SE0 PBT 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Melt Flow | 42 g/10 min @Load 5.00 kg, Temperature 250 °C |
42 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 420SE0 PBT (Asia Pacific) 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Melt Flow | 42 g/10 min @Load 5.00 kg, Temperature 250 °C |
42 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® 420SE0 PBT (Europe-Africa-Middle East) 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Melt Flow | 42 g/10 min @Load 2.16 kg, Temperature 380 °C |
42 g/10 min @Load 4.76 lb, Temperature 716 °F |
ASTM D1238 |
Solvay Specialty Polymers Veradel® 3400 Polyethersulfone (PESU) Veradel® 3400 polyethersulfone (PESU) is a high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam,.. |
|||
Melt Flow | 42 g/10 min @Load 10.0 kg, Temperature 220 °C |
42 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® VG-4920F ABS, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 42 g/10 min @Load 10.0 kg, Temperature 220 °C |
42 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® VG-4920F ABS, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 42 g/10 min @Load 3.80 kg, Temperature 200 °C |
42 g/10 min @Load 8.38 lb, Temperature 392 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL FP3060 PPE+PS (Europe-Africa-Middle East) Noryl* FP3060 is an unfilled, injection moldable modified polyphenylene ether resin. Designed for good dimensional stability and high flow , this resin also uses non-chlorinated, non-brominated FR .. |
|||
Melt Flow | 42 g/10 min @Load 2.16 kg, Temperature 230 °C |
42 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPH 10012 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 10012 is a nucleated and antistatic homopolymer polypropylene obtained by controlled rheology.ApplicationPPH 10012 is intended for high speed injection molding of household.. |
|||
Melt Flow | 42 g/10 min @Load 1.00 kg, Temperature 235 °C |
42 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Diamond Polymers Softflex® SF 0450 Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 42 g/10 min @Load 2.16 kg |
42 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 8.5. |
Dow DOWLEX™ IP-42 High Density Polyethylene DOWLEX® IP-42 resin is an improved processing high density polyethylene resin designed for excellent flow and high impact. DOWLEX IP-42 resin is designed by optimizing the breadth and shape of the .. |
|||
Melt Flow | 42 g/10 min @Load 2.16 kg, Temperature 235 °C |
42 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AMN P20 TLD Nylon 12, Flexible, Injection Grade (Conditioned) Designation ISO 1874-PA12-P,MHLR,14-005Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and .. |
|||
Melt Flow | 42 g/10 min @Load 2.16 kg, Temperature 235 °C |
42 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Rilsan® AMN P20 TLD Nylon 12, Flexible, Injection Grade (Dry) Designation ISO 1874-PA12-P,MHLR,14-005Flexible grade for injection molding. Available colors: black and natural. Light and heat stabilized. Mold-release agent.Good impact strength. Flexibility and .. |
|||
Melt Flow | 42 g/10 min @Load 10.0 kg, Temperature 220 °C |
42 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron IM-11BM ABS Injection Molding Grade High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali |
|||
Melt Flow | 42 g/10 min @Load 10.0 kg, Temperature 220 °C |
42 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron TG-3(M) ABS High Impact Injection Molding Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali |
|||
Melt Flow | 42 g/10 min @Load 10.0 kg, Temperature 220 °C |
42 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron IM-11BM ABS Injection Molding Grade High Impact Strength, Medium Flow, High Fatigue ResistanceInformation provided by Bhansali |
|||
Melt Flow | 42 g/10 min @Load 10.0 kg, Temperature 220 °C |
42 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D-1238 |
Bhansali Engineering Abstron TG-3(M) ABS High Impact Injection Molding Very High & Medium Impact, Paintable Automotive Grades Information provided by Bhansali |
|||
Melt Flow | 42 g/10 min @Load 2.16 kg, Temperature 230 °C |
42 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
E-Polymers EFLEX® S1030 General S-series ( SBS, SEBS compound resins): E-FLEX S series resins are based on SBS/SEBS/SEEPS/PP exhibiting excellent high and low temperature resistance and easy processing with conventional thermoplas.. |
|||
Melt Flow | 42 - 49 g/10 min @Load 2.16 kg, Temperature 235 °C |
42 - 49 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238 |
Gromax PBT 1200-211M Product Description: PBT unreinforced middle viscosity injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Exce.. |
|||
Melt Flow | 42 g/10 min | 42 g/10 min | ISO 1133 |
LyondellBasell INDURE™ X210 TPO Description: INDURE™ X210 engineered polyolefin material is designed for large automotive exterior applications that require ductile impact properties at low temperatures, and processability. Appli.. |