Solvay Engineered Polymers SEQUEL® 1405 TPO  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO) , Polyolefin
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Engineered Polymers SEQUEL® 1405 TPO  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: SEQUEL® 1405 engineered polyolefin material is designed for automotive exterior applications that require a combination of stiffness, low-temperature impact resistance, high flow and excellent processability. Applications: Bumper fascias and other large components that must exhibit durable paintability or excellent weatherability. Information provided by Solvay Engineered Polymers.LyondellBasell acquired Solvay Engineered Polymers in 2008. This grade is not part of the current LyondellBasell product line.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
ISO 1183
Linear Mold Shrinkage 0.011 - 0.013 cm/cm
0.011 - 0.013 in/in
after bake, 120°C for 1 hr.; ISO 294
Melt Flow 42 g/10 min
42 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.0 MPa
2470 psi
150x10x4 mm specimen, 50 mm/min; ISO 527-1/527-2
Flexural Modulus 1.50 GPa
218 ksi
80x10x4 mm specimen, 2 mm/min; ISO 178
Impact Test 40.6 J
29.9 ft-lb
multiaxial, 2.2 m/s; ASTM D3763