Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 430 - 550 g/10 min @Load 2.16 kg, Temperature 275 °C |
430 - 550 g/10 min @Load 4.76 lb, Temperature 527 °F |
ASTM D1238 |
Solvay Specialty Polymers Halar® 1400LC Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**) Information provided by Solvay Specialty Polymers. |
|||
Melt Flow | 430 g/10 min @Load 5.00 kg, Temperature 316 °C |
430 g/10 min @Load 11.0 lb, Temperature 600 °F |
ASTM D1283 |
Chevron Phillips Ryton® PR34 Polyphenylene Sulfide Resin
(discontinued **) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Melt Flow | 430 - 550 g/10 min @Load 2.16 kg, Temperature 275 °C |
430 - 550 g/10 min @Load 4.76 lb, Temperature 527 °F |
ASTM D1238 |
Solvay Specialty Polymers Halar® 1400LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Low ViscosityUses: FibersAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 300 °CInformation provided by Solvay Spec.. |