Melt Flow 430 - 550 g/10 min

@Load 2.16 kg,
Temperature 275 °C
430 - 550 g/10 min

@Load 4.76 lb,
Temperature 527 °F
ASTM D1238
Solvay Specialty Polymers Halar® 1400LC Polyethylene, Chlorotrifluoroethylene (ECTFE)  (Unverified Data**)
Information provided by Solvay Specialty Polymers.
Melt Flow 1.00 - 550 g/10 min
1.00 - 550 g/10 min
Average value: 31.9 g/10 min Grade Count:22
Overview of materials for ECTFE Fluoropolymer
This property data is a summary of similar materials in the MatWeb database for the category "ECTFE Fluoropolymer". Each property range of values reported is minimum and maximum values of appropriat..
Melt Flow 430 - 550 g/10 min

@Load 2.16 kg,
Temperature 275 °C
430 - 550 g/10 min

@Load 4.76 lb,
Temperature 527 °F
ASTM D1238
Solvay Specialty Polymers Halar® 1400LC Ethylene Chlorotrifluoroethylene Copolymer (ECTFE)
Low ViscosityUses: FibersAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 300 °CInformation provided by Solvay Spec..