Physical Properties Metric English Comments
Melt Flow 3.00 - 44.0 g/10 min
3.00 - 44.0 g/10 min
Average value: 15.4 g/10 min Grade Count:106
Overview of materials for Polycarbonate/PET Polyester Blend
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values..