Physical Properties Metric English Comments
Melt Flow 2.00 - 44.4 g/10 min
2.00 - 44.4 g/10 min
Average value: 19.4 g/10 min Grade Count:5
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..