Physical Properties Metric English Comments
Melt Flow 0.300 - 45.0 g/10 min
0.300 - 45.0 g/10 min
Average value: 15.9 g/10 min Grade Count:42
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
Melt Flow 1.00 - 45.0 g/10 min
1.00 - 45.0 g/10 min
Average value: 25.3 g/10 min Grade Count:4
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..
Melt Flow 2.00 - 45.0 g/10 min
2.00 - 45.0 g/10 min
Average value: 17.3 g/10 min Grade Count:3
Overview of materials for Nylon 66/6, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are incl..
Melt Flow 15.0 - 45.0 g/10 min

@Load 10.0 kg,
Temperature 190 °C
15.0 - 45.0 g/10 min

@Load 22.0 lb,
Temperature 374 °F
ASTM D1238
Teknor Apex Sinpolene MBB3462 Low Density Polyethylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (400000 ppm) Features: General Purpose Uses: Non-specific Food Applications Forms: Pellets Pro..
Melt Flow 20.0 - 45.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20.0 - 45.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Sinpolene MBW1994 Polypropylene
Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (500000 ppm) Forms: Pellets Features: General PurposeInformation Provided by Teknor ..
Melt Flow 1.20 - 45.0 g/10 min
1.20 - 45.0 g/10 min
Average value: 13.5 g/10 min Grade Count:24
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Plating Grade
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Plating Grade". Each property range of values reported is minimum..
Melt Flow 3.00 - 45.0 g/10 min
3.00 - 45.0 g/10 min
Average value: 13.8 g/10 min Grade Count:6
Overview of materials for Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant". Each property range of values re..