Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.05 - 1.16 g/cc
0.0379 - 0.0419 lb/in³
Average value: 1.09 g/cc Grade Count:40
Water Absorption 0.300 - 1.00 %
0.300 - 1.00 %
Average value: 0.575 % Grade Count:6
Moisture Absorption at Equilibrium 0.350 - 0.700 %
0.350 - 0.700 %
Average value: 0.450 % Grade Count:5
Viscosity 350000 - 600000 cP

@Temperature 220 - 220 °C
350000 - 600000 cP

@Temperature 428 - 428 °F
Average value: 475000 cP Grade Count:2
Linear Mold Shrinkage 0.00300 - 0.0140 cm/cm
0.00300 - 0.0140 in/in
Average value: 0.00582 cm/cm Grade Count:27
Melt Flow 0.300 - 45.0 g/10 min
0.300 - 45.0 g/10 min
Average value: 15.9 g/10 min Grade Count:42
Mechanical Properties Metric English Comments
Hardness, Rockwell R 78.0 - 116
78.0 - 116
Average value: 107 Grade Count:31
Ball Indentation Hardness 70.0 - 95.0 MPa
10200 - 13800 psi
Average value: 80.0 MPa Grade Count:5
Tensile Strength, Ultimate 29.0 - 51.0 MPa
4210 - 7400 psi
Average value: 39.7 MPa Grade Count:14
Tensile Strength, Yield 30.4 - 55.9 MPa
4410 - 8110 psi
Average value: 44.4 MPa Grade Count:35
Elongation at Break 10.0 - 70.0 %
10.0 - 70.0 %
Average value: 32.7 % Grade Count:30
Elongation at Yield 3.50 - 6.00 %
3.50 - 6.00 %
Average value: 4.33 % Grade Count:12
Modulus of Elasticity 1.90 - 2.06 GPa
276 - 299 ksi
Average value: 1.98 GPa Grade Count:9
Flexural Yield Strength 47.1 - 92.2 MPa
6830 - 13400 psi
Average value: 67.2 MPa Grade Count:34
Flexural Modulus 1.37 - 2.76 GPa
199 - 400 ksi
Average value: 2.09 GPa Grade Count:36
Izod Impact, Notched 0.0981 - 3.04 J/cm
0.184 - 5.70 ft-lb/in
Average value: 1.24 J/cm Grade Count:36
0.600 - 1.30 J/cm

@Temperature -30.0 - 0.000 °C
1.12 - 2.44 ft-lb/in

@Temperature -22.0 - 32.0 °F
Average value: 0.875 J/cm Grade Count:2
0.600 - 1.30 J/cm

@Thickness 3.17 - 3.17 mm
1.12 - 2.44 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 0.875 J/cm Grade Count:2
Izod Impact, Unnotched 0.392266 - 0.392266 J/cm

@Temperature -30.0 - -30.0 °C
0.734875 - 0.734875 ft-lb/in

@Temperature -22.0 - -22.0 °F
Average value: 0.392 J/cm Grade Count:1
0.392266 - 0.392266 J/cm

@Thickness 3.20 - 6.40 mm
0.734875 - 0.734875 ft-lb/in

@Thickness 0.126 - 0.252 in
Average value: 0.392 J/cm Grade Count:1
Charpy Impact Unnotched 5.10 - 18.0 J/cm²
24.3 - 85.7 ft-lb/in²
Average value: 11.7 J/cm² Grade Count:6
7.00 - 12.0 J/cm²

@Temperature -30.0 - -30.0 °C
33.3 - 57.1 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 8.60 J/cm² Grade Count:5
Charpy Impact, Notched 0.500 - 1.40 J/cm²
2.38 - 6.66 ft-lb/in²
Average value: 0.850 J/cm² Grade Count:8
0.200 - 0.700 J/cm²

@Temperature -30.0 - -20.0 °C
0.952 - 3.33 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 0.283 J/cm² Grade Count:6
Thermal Properties Metric English Comments
CTE, linear 80.0 - 121 µm/m-°C
44.4 - 67.2 µin/in-°F
Average value: 103 µm/m-°C Grade Count:9
Maximum Service Temperature, Air 75.0 - 90.0 °C
167 - 194 °F
Average value: 86.0 °C Grade Count:5
Deflection Temperature at 0.46 MPa (66 psi) 80.0 - 94.0 °C
176 - 201 °F
Average value: 91.1 °C Grade Count:10
Deflection Temperature at 1.8 MPa (264 psi) 65.0 - 96.0 °C
149 - 205 °F
Average value: 83.3 °C Grade Count:31
Vicat Softening Point 86.0 - 106 °C
187 - 223 °F
Average value: 95.1 °C Grade Count:15
Glass Transition Temp, Tg 107 °C
225 °F
Average value: 107 °C Grade Count:3
UL RTI, Electrical 50.0 - 60.0 °C
122 - 140 °F
Average value: 52.7 °C Grade Count:7
UL RTI, Mechanical with Impact 50.0 - 60.0 °C
122 - 140 °F
Average value: 52.7 °C Grade Count:7
UL RTI, Mechanical without Impact 50.0 - 60.0 °C
122 - 140 °F
Average value: 52.7 °C Grade Count:7
Flammability, UL94 HB - V-2
HB - V-2
Grade Count:30
Optical Properties Metric English Comments
Refractive Index 1.52 - 1.54
1.52 - 1.54
Average value: 1.53 Grade Count:4
Haze 1.70 - 11.0 %
1.70 - 11.0 %
Average value: 3.88 % Grade Count:22
Transmission, Visible 78.0 - 90.0 %
78.0 - 90.0 %
Average value: 87.1 % Grade Count:36
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+11 - 1.00e+16 ohm-cm
1.00e+11 - 1.00e+16 ohm-cm
Average value: 1.38e+15 ohm-cm Grade Count:8
Surface Resistance 1.00e+11 - 1.00e+15 ohm
1.00e+11 - 1.00e+15 ohm
Average value: 4.52e+14 ohm Grade Count:9
Dielectric Constant 2.80 - 3.00
2.80 - 3.00
Average value: 2.88 Grade Count:5
Dielectric Strength 7.00 - 37.0 kV/mm
178 - 940 kV/in
Average value: 26.0 kV/mm Grade Count:3
Dissipation Factor 0.0130 - 0.0160
0.0130 - 0.0160
Average value: 0.0148 Grade Count:5
Processing Properties Metric English Comments
Processing Temperature 190 - 265 °C
374 - 509 °F
Average value: 223 °C Grade Count:5
Nozzle Temperature 200 - 260 °C
392 - 500 °F
Average value: 221 °C Grade Count:7
Adapter Temperature 235 - 245 °C
455 - 473 °F
Average value: 240 °C Grade Count:4
Die Temperature 113 - 118 °C
235 - 245 °F
Average value: 116 °C Grade Count:4
Melt Temperature 180 - 260 °C
356 - 500 °F
Average value: 222 °C Grade Count:16
Mold Temperature 40.0 - 90.0 °C
104 - 194 °F
Average value: 60.2 °C Grade Count:16
Injection Velocity 60.0 - 200 mm/sec
2.36 - 7.87 in/sec
Average value: 107 mm/sec Grade Count:3
Roll Temperature 75.0 - 95.0 °C
167 - 203 °F
Average value: 85.0 °C Grade Count:4
Drying Temperature 70.0 - 88.0 °C
158 - 190 °F
Average value: 77.4 °C Grade Count:11
Moisture Content 0.100 - 0.700 %
0.100 - 0.700 %
Average value: 0.500 % Grade Count:3
Injection Pressure 4.83 - 150 MPa
700 - 21800 psi
Average value: 73.3 MPa Grade Count:10