Physical Properties Metric English Comments
Melt Flow 46 - 50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
46 - 50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A Condition L; ASTM D1238
Network Polymers NPP 50-5052
Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.
Melt Flow 46 g/10 min

@Load 2.16 kg,
Temperature 330 °C
46 g/10 min

@Load 4.76 lb,
Temperature 626 °F
ASTM D1238
SABIC Innovative Plastics Lexan® FXM2143H PC Copolymer
FXM2143H is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C.
Melt Flow 46 g/10 min

@Load 2.16 kg,
Temperature 330 °C
46 g/10 min

@Load 4.76 lb,
Temperature 626 °F
ASTM D1238
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer
XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Melt Flow 46 g/10 min

@Load 2.16 kg,
Temperature 330 °C
46 g/10 min

@Load 4.76 lb,
Temperature 626 °F
ASTM D1238
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Asia Pacific)
XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Melt Flow 46 g/10 min

@Load 2.16 kg,
Temperature 330 °C
46 g/10 min

@Load 4.76 lb,
Temperature 626 °F
ASTM D1238
SABIC Innovative Plastics Lexan® XHT2141 PC Copolymer (Europe-Africa-Middle East)
XHT2141 is a high flow, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Melt Flow 46 g/10 min

@Load 2.16 kg,
Temperature 330 °C
46 g/10 min

@Load 4.76 lb,
Temperature 626 °F
ASTM D1238
SABIC Innovative Plastics Lexan® XHT2143 PC Copolymer (Europe-Africa-Middle East)
XHT2143 is a high flow, UV stabilized, high heat polycarbonate copolymer with an HDT/Af of 142 C. It is available in a range of opaque and limited transparent colors.
Melt Flow 46 g/10 min

@Load 2.16 kg,
Temperature 330 °C
46 g/10 min

@Load 4.76 lb,
Temperature 626 °F
ASTM D1238
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer
XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo..
Melt Flow 46 g/10 min

@Load 2.16 kg,
Temperature 330 °C
46 g/10 min

@Load 4.76 lb,
Temperature 626 °F
ASTM D1238
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Europe-Africa-Middle East)
XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo..
Melt Flow 46 g/10 min

@Load 5.00 kg,
Temperature 190 °C
46 g/10 min

@Load 11.0 lb,
Temperature 374 °F
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 57 Shore A  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 60..
Melt Flow 46 g/10 min

@Load 2.16 kg,
Temperature 330 °C
46 g/10 min

@Load 4.76 lb,
Temperature 626 °F
ASTM D1238
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Asia Pacific)
XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo..
Melt Flow 46 g/10 min

@Load 2.16 kg,
Temperature 320 °C
46 g/10 min

@Load 4.76 lb,
Temperature 608 °F
ASTM D1238
Kuraray Genestarâ„¢ G1302 Nylon, 30% Glass Filled
Abrasion Resistance HB grade. Halogen free, following the standards that Br is less than 900ppm, Cl is less than 900ppm, and total of halogen amount (Br and Cl) is less than 1500ppm. It delivers low..
Melt Flow 46 g/10 min

@Load 10.0 kg,
Temperature 220 °C
46 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Samsung Cheil Industries Infino® GC-1017 PC/ABS, FR
Information provided by Samsung Cheil Industries.
Melt Flow 46 g/10 min

@Load 10.0 kg,
Temperature 220 °C
46 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Samsung Cheil Industries Infino® NH-1017D PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Melt Flow 46 g/10 min

@Load 10.0 kg,
Temperature 220 °C
46 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Samsung Cheil Industries Infino® NH-1017D PC/ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
Melt Flow 46 g/10 min

@Load 10.0 kg,
Temperature 220 °C
46 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Samsung Cheil Industries Infino® GC-1017 PC/ABS, FR
Information provided by Samsung Cheil Industries.
Melt Flow 46 g/10 min

@Load 5.00 kg,
Temperature 200 °C
46 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Teknor Apex TEKBOND® 6000-75 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Melt Flow 46 g/10 min

@Load 2.16 kg,
Temperature 330 °C
46 g/10 min

@Load 4.76 lb,
Temperature 626 °F
ISO 1133
Covestro Apec® 1697 High-Heat Polycarbonate
This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along..
Melt Flow 46 - 54 g/10 min

@Load 2.16 kg,
Temperature 230 °C
46 - 54 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
AKG Polymers Vision PP PPC BL5005 Polypropylene Copolymer Compound
Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin..
Melt Flow 46 - 54 g/10 min

@Load 2.16 kg,
Temperature 230 °C
46 - 54 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
AKG Polymers Vision PP PPH BL5003 Polypropylene Homopolymer Compound
Vision consists of a complete assortment of high-quality compounds based on industrial PP waste.Applications: Automotive, Non-food packaging, Storage/transport systems, Road and hydraulic Engineerin..
Melt Flow 46 g/10 min

@Load 14.91 kg,
Temperature 175 °C
46 g/10 min

@Load 32.87 lb,
Temperature 347 °F
ASTM D-1238
Axiall 1701 Clear 7002 Flexible PVC
Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation ..