Network Polymers NPP 50-5052

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Network Polymers
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Network Polymers NPP 50-5052.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.
Physical Properties Metric English Comments
Density 0.952 g/cc
0.0344 lb/in³
ASTM D1505
Melt Flow 46 - 50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
46 - 50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 24.8 MPa
3600 psi
chs 2 in/min; ASTM D638
Elongation at Break 4.0 %
4.0 %
chs 2 in/min; ASTM D638
Flexural Modulus 1.07 GPa
155 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Users viewing this material also viewed the following: