Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.00 - 9.00 g/10 min | 5.00 - 9.00 g/10 min | Average value: 7.92 g/10 min Grade Count:6 |
Overview of materials for Acetal Copolymer, Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Melt Flow | 5.00 g/10 min @Load 1.00 kg, Temperature 235 °C |
5.00 g/10 min @Load 2.20 lb, Temperature 455 °F |
ASTM D1238 |
Teknor Apex Chemlon® 253 Nylon 6, Toughened Features: Medium Impact Resistance; Impact modified co-polymer grade offering strength and flexibility, especially at low temperatures Processing Method: Injection Molding Forms: PelletsInformation .. |
|||
Melt Flow | 5.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1061 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 5.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 2860E Thermoplastic Elastomer Notes: Translucent Features: Good Chemical and Oil Resistance; Tough; Good Melt StrengthInformation Provided by Teknor Apex |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 9000 Thermoplastic Elastomer Notes: Translucent Features: High FlowInformation Provided by Teknor Apex |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1766 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1907E CLR Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2357-A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 5.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1544 Thermoplastic Elastomer Notes: Translucent Features: Good Chemical and Oil ResistanceInformation Provided by Teknor Apex |
|||
Melt Flow | 5.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1351J Thermoplastic Elastomer Uses: Consumer Applications; Gaskets; Plumbing Parts; Pump Parts Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Drying is not necessary. However, if moisture is a p.. |
|||
Melt Flow | 5.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2745 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 5.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2755 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 5.00 g/10 min @Load 10.0 kg, Temperature 190 °C |
5.00 g/10 min @Load 22.0 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB006LE Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (400000 ppm) Features: General Purpose Uses: Film Forms: Pellets Processing Method: Blow Moldi.. |
|||
Melt Flow | 5.00 g/10 min @Load 10.0 kg, Temperature 190 °C |
5.00 g/10 min @Load 22.0 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB1061 Linear Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (450000 ppm) Features: General Purpose Uses: Film Forms: Pellets Processing Method: Blow Moldin.. |
|||
Melt Flow | 5.00 - 15.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 - 15.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW1781 Linear Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (600000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor.. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TELC 302 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 5.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1642E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-4145 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 5.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
5.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-8712R Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2470A Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Uniprene® UN-2420A Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Melt Flow | 5.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil HDP8760.29 Rotational Molding Resin Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal.. |
|||
Melt Flow | 5.00 g/10 min @Load 10.0 kg, Temperature 220 °C |
5.00 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron KU602L ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Melt Flow | 5.00 g/10 min @Load 10.0 kg, Temperature 220 °C |
5.00 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron KU670 ABS Heat Resistant Ultra Super High heat ResistantInformation provided by Bhansali |
|||
Melt Flow | 5.00 - 58.4 g/10 min | 5.00 - 58.4 g/10 min | Average value: 16.9 g/10 min Grade Count:14 |
Overview of materials for Acetal Copolymer, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Melt Flow | 5.00 - 50.0 g/10 min | 5.00 - 50.0 g/10 min | Average value: 22.7 g/10 min Grade Count:3 |
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are .. |
|||
Melt Flow | 5.00 - 65.0 g/10 min | 5.00 - 65.0 g/10 min | Average value: 16.8 g/10 min Grade Count:6 |
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% .. |
|||
Melt Flow | 5.00 - 21.0 g/10 min | 5.00 - 21.0 g/10 min | Average value: 15.0 g/10 min Grade Count:10 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass Filler". Each property range of values reported is minimum and .. |
|||
Melt Flow | 5.00 - 23.0 g/10 min | 5.00 - 23.0 g/10 min | Average value: 12.0 g/10 min Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Filled, Impact Modified". Each property range of values reported.. |