Polymer Property : Melt Flow = 5.885 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 5.885 g/10 min

@Load 10.0 kg,
Temperature 220 °C
5.885 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Styrolution Luran® S 797 S UV White 33999 Q455 ASA
Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN..
Melt Flow 5.885 g/10 min

@Load 10.0 kg,
Temperature 220 °C
5.885 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Styrolution Luran® S 797 S White 35962 ASA
Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN..