Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.885 g/10 min @Load 10.0 kg, Temperature 220 °C |
5.885 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Luran® S 797 S UV White 33999 Q455 ASA Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Melt Flow | 5.885 g/10 min @Load 10.0 kg, Temperature 220 °C |
5.885 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Luran® S 797 S White 35962 ASA Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |