Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 53.55 g/10 min @Load 5.00 kg, Temperature 260 °C |
53.55 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Styrolution Luran® S KR 2867 C WU Colored ASA+PC Description: Easy flowing injection molding grade containing bromine-, chlorine- and antimony-free flame retardant.Information provided by STYROLUTION, which is a joint venture between BASF and INEO.. |