Polymer Property : Melt Flow = 53.55 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 53.55 g/10 min

@Load 5.00 kg,
Temperature 260 °C
53.55 g/10 min

@Load 11.0 lb,
Temperature 500 °F
ISO 1133
Styrolution Luran® S KR 2867 C WU Colored ASA+PC
Description: Easy flowing injection molding grade containing bromine-, chlorine- and antimony-free flame retardant.Information provided by STYROLUTION, which is a joint venture between BASF and INEO..