Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.5 - 6.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.5 - 6.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Kraton® D1163 J (SIS) Linear Block Copolymer Description: Kraton D1163 J Polymer is a clear, linear block copolymer based on styrene and isoprene with bound styrene of 15% mass. It is supplied from Japan in the physical form(s) identified in t.. |