Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 72 g/10 min @Load 2.16 kg, Temperature 190 °C |
72 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Sclair® 2316 LLDPE Injection Molding Resin Features: Low odor, low warpage, fast cycling, high surface gloss, permits light weight lid design.Data provided by the manufacturer. |
|||
Melt Flow | 72 g/10 min @Pressure 0.655 MPa |
72 g/10 min @Pressure 95.0 psi |
Severs Efflux; Geon® ALTC 23 (with provided formulation); Internal Method |
PolyOne Geon™ 120 Series 121A Polyvinyl Chloride Homopolymer (PVC Homopolymer) Geon® 121A is high molecular weight resin providing good fused film physical properties. It provides good chemical foamability for producing medium to high density foams. It gives good dispersabili.. |
|||
Melt Flow | 72 g/10 min | 72 g/10 min | ASTM D1238 |
Flint Hills P9G8Z-036 Polypropylene Specialty Polypropylene Features: Broad MWD Homopolymer. Product does not contain animal derived components. Phthalate-free.Applications: Extrusion coatingInformation Provided by Flint Hills Resources |
|||
Melt Flow | 72 g/10 min @Load 2.16 kg, Temperature 230 °C |
72 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
BASF Novolen® 1148 TC Polypropylene Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Melt Flow | 72 g/10 min | 72 g/10 min | |
Cathay Terryl® Renewable Engineering Polyamide Terryl® provides significant advantages in spinnability, dyeability, water absorption and comfort.Information provided by Cathay |