Cathay Terryl® Renewable Engineering Polyamide

Category Polymer , Thermoplastic , Nylon
Manufacturer Cathay Industrial Biotech
Trade Name Terryl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cathay Terryl® Renewable Engineering Polyamide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Terryl® provides significant advantages in spinnability, dyeability, water absorption and comfort.Information provided by Cathay
Physical Properties Metric English Comments
Molecular Weight 20000 - 60000 g/mol
20000 - 60000 g/mol
Melt Flow 72 g/10 min
72 g/10 min
Mechanical Properties Metric English Comments
Elongation at Break 50 %
50 %
Tenacity 0.300 - 0.500 N/tex
3.40 - 5.66 g/denier
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
Descriptive Properties Value Comments
Dyeability 25.5 L Value
100°C
30.5 L Value
40°C
Elastic Recovery fiber 10%
97-100%
fiber 30%
60-65%
Fiber moisture regain 5-6%