Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 91 g/10 min @Load 2.16 kg, Temperature 230 °C |
91 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flex® A 6041 Clear TPE Thermoplastic Elastomer This material bonds to polypropylene.Forms:PelletsProcessing Method:Injection Molding Information provided by Multibase |
|||
Melt Flow | 91 g/10 min @Load 2.16 kg, Temperature 230 °C |
91 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flex® A 7041 Clear TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |