Physical Properties Metric English Comments
Melt Flow 92.25 g/10 min

@Load 5.00 kg,
Temperature 275 °C
92.25 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Conditioned)
Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov..
Melt Flow 92.25 g/10 min

@Load 5.00 kg,
Temperature 275 °C
92.25 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® B3EG3 15% Glass Filled PA6 (Dry)
Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov..
Melt Flow 92.25 g/10 min

@Load 5.00 kg,
Temperature 275 °C
92.25 g/10 min

@Load 11.0 lb,
Temperature 527 °F
ISO 1133
BASF Ultramid® B3EG3 BK 00564 15% Glass Filled PA6 (Conditioned)
Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov..