Polymer Property : Cell Length = 0.350 mm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Cell Length 0.350 mm
0.0138 in
Typical Diameter
Zotefoams Evazote® EV50 Ethylene Vinyl Acetate Copolymer Foam
Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta..
Cell Length 0.350 mm
0.0138 in
Typical Diameter
Zotefoams Plastazote® LD15FM Low Density Polyethylene Foam, Flame Retarded
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Cell Length 0.350 - 0.900 mm
0.0138 - 0.0354 in
Zotefoams Plastazote® LD60 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Cell Length 0.350 - 0.900 mm
0.0138 - 0.0354 in
Zotefoams Plastazote® LD70 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Cell Length 0.350 mm
0.0138 in
Typical Diameter
Zotefoams Plastazote® MP33 Metallocene Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..