Polymer Property : Thickness = 0.0492 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 0.890 - 1.25 microns
0.0350 - 0.0492 mil
2000-4000 rpm
Dow SiLK™ I 1070 Semiconductor Dielectric Resin
SiLK™ I 1070 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I 1070 is compatible wi..