Polymer Property : Thickness = 0.0700 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 0.0700 - 0.100 microns
0.00276 - 0.00394 mil
Dow SiLK™ Y 80 Semiconductor Dielectric Resin
SiLK™ Y 80 has an average pore size of < 2nm and a range of 1-3 nm, porous SiLK™ resins enables continuous Tantulum PVD barriers for 65 nm technology and beyond. Information provided by Dow