Polymer Property : Thickness = 0.236 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 2.00 - 6.00 microns
0.0787 - 0.236 mil
General plating (excluding exotic metals)
Parker Chomerics SPRING-LINE® Beryllium-Copper Gasket
Description: SPRING-LINE beryllium-copper gaskets combine high levels of EMI shielding effectiveness with spring-finger wiping and low closure force properties. The high performance qualities of ber..
Thickness 2.00 - 6.00 microns
0.0787 - 0.236 mil
Eifeler Coatings Technology CrCN PVD Coating
Key Characteristics: low stress / good adhesion, high toughness and corrosion resistancePrimary Applications: drawing, pressing, bending and stamping of copper and other non-ferrous materials; metal..
Thickness 2.00 - 6.00 microns
0.0787 - 0.236 mil
Eifeler Coatings Technology CrN PVD Coating
Key Characteristics: low stress / good adhesion, high toughness and corrosion resistancePrimary Applications: drawing, pressing, bending and stamping of copper and other non-ferrous materials; metal..
Thickness 0.100 - 6.00 microns
0.00394 - 0.236 mil
Coating Thickness
BACT Dylyn® Diamond-Like Nanocomposite Coating
a-C:H/a-Si:O nanocomposite. This coating provides the lowest friction of the BACT products, even in high humidity or wet environments. It offers an excellent combination of anti-stick and wear be..