Polymer Property : Thickness = 104 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 104 microns
4.10 mil
ASTM D3652
3M 4179 (Clear) Polyethylene Protective Tapes
3M™ Polyethylene Protective Tapes 4179 has a very high-tack adhesive system to help provide temporary protection of many dissimilar metals, automotive carpeting, carpeted door panels and plastic sc..
Thickness 104 microns
4.10 mil
Backing; ASTM D3652
3M 471 Vinyl Tape
3M™ Vinyl Tape 471 is a conformable colored (9 colors plus transparent) tapes made from vinyl backing with rubber adhesive. They are ideal for many lane and safety markings, color coding, abrasion ..
Thickness 104 microns
4.10 mil
Backing; ASTM D3652
3M 4712 Vinyl Tape
3M™ Vinyl Tape 4712 is a conformable colored (9 colors plus transparent) tapes made from vinyl backing with rubber adhesive. They are ideal for many lane and safety markings, color coding, abrasion..
Thickness 104 microns
4.10 mil
Total; ASTM D3752
3M 396 Super Bond Film
3M™ Super Bond Film Tape 396 is a polyester film tape for adhering to polyesters, polyethylenes and many other difficult-to-adhere-to surfaces.Information provided by 3M