Physical Properties Metric English Comments
Thickness 427 microns
16.8 mil
Typical; TAPPI-411
DuPont™ Nomex® 411 Paper, 15 mil Nominal Thickness
Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil..