Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 427 microns | 16.8 mil | Typical; TAPPI-411 |
DuPont™ Nomex® 411 Paper, 15 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |