Thickness 2000 microns
78.7 mil
SMAC SMACWRAP® ST Damping Material, 0.20 mm
SMACWRAP® concept is a smart and lightweight solution to embed into composite structures a very thin viscoelastic material. The SMACWRAP® will then bring damping to the composite structure wit..
Thickness 2000 microns
78.7 mil
Thickness tested
Thermoseal KLINGER® top-chem-2003 PTFE Gasketing
Ideal for low bolt applications or w here flanges are delicateExcellent chemical resistance to acidic and alkaline attackHighly compressibleFDA compatibleIdeal for higher temperatures and pressuresH..
Thickness 2000 microns
78.7 mil
ASTM D374, method D, using 17 N/cm²
DuPont™ Nomex® Type 993, 80 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard
Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ..
Thickness <= 2000 microns
<= 78.7 mil
Multiple coats
Daikin NEOFLON NC-1539 FEP Coating Powder, Gray
NEOFLON FEP coating powders are designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: Multiple coats, up to 2,000 microns.Processing Method..
Thickness 2000 microns
78.7 mil
American Computer Optics High Transmission Filter 2 mm
Maximum Size: 48" X 84"Abrasion: MIL-C-675C, section 4.5.11Adhesion: MIL-C-48497A, para 4.5.3.1Humidity: The coated optical surface will show no signs of deterioration after a 24 hour humidity expo..
Thickness 2000 microns
78.7 mil
American Computer Optics Water White Filter 2 mm
Maximum Size: 48" X 84"Abrasion: MIL-C-675C, section 4.5.11Adhesion: MIL-C-48497A, para 4.5.3.1Humidity: The coated optical surface will show no signs of deterioration after a 24 hour humidity expo..
Thickness 2000 microns
78.7 mil
American Computer Optics Water White Filter 2 mm Single-Sided
Maximum Size: 75" X 110"Abrasion: MIL-C-675C, section 4.5.11Adhesion: MIL-C-48497A, para 4.5.3.1Humidity: The coated optical surface will show no signs of deterioration after a 24 hour humidity exp..
Thickness 2000 microns
78.7 mil
American Computer Optics UV Protection Glass 2 mm
Maximum Size: 24" X 36"Abrasion: MIL-C-675C, section 4.5.11Adhesion: MIL-C-48497A, para 4.5.3.1Humidity: The coated optical surface will show no signs of deterioration after a 24 hour humidity expo..
Thickness 2000 microns
78.7 mil
Mo-Sci Corporation GA-80-N Green Filter Glass
Applications: Lead-free NVIS green filter glass for Nichia White LED sources.Information provided by Mo-Sci Corporation.
Thickness 2000 microns
78.7 mil
SMAC SMACWRAP® EX Damping Material, 0.20 mm
SMACWRAP® concept is a smart and lightweight solution to embed into composite structures a very thin viscoelastic material. The SMACWRAP® will then bring damping to the composite structure without..