Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 2000 microns | 78.7 mil | |
SMAC SMACWRAP® ST Damping Material, 0.20 mm SMACWRAP® concept is a smart and lightweight solution to embed into composite structures a very thin viscoelastic material. The SMACWRAP® will then bring damping to the composite structure wit.. |
|||
Thickness | 2000 microns | 78.7 mil | Thickness tested |
Thermoseal KLINGER® top-chem-2003 PTFE Gasketing Ideal for low bolt applications or w here flanges are delicateExcellent chemical resistance to acidic and alkaline attackHighly compressibleFDA compatibleIdeal for higher temperatures and pressuresH.. |
|||
Thickness | 2000 microns | 78.7 mil | ASTM D374, method D, using 17 N/cm² |
DuPont™ Nomex® Type 993, 80 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |
|||
Thickness | <= 2000 microns | <= 78.7 mil | Multiple coats |
Daikin NEOFLON NC-1539 FEP Coating Powder, Gray NEOFLON FEP coating powders are designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: Multiple coats, up to 2,000 microns.Processing Method.. |
|||
Thickness | 2000 microns | 78.7 mil | |
American Computer Optics High Transmission Filter 2 mm Maximum Size: 48" X 84"Abrasion: MIL-C-675C, section 4.5.11Adhesion: MIL-C-48497A, para 4.5.3.1Humidity: The coated optical surface will show no signs of deterioration after a 24 hour humidity expo.. |
|||
Thickness | 2000 microns | 78.7 mil | |
American Computer Optics Water White Filter 2 mm Maximum Size: 48" X 84"Abrasion: MIL-C-675C, section 4.5.11Adhesion: MIL-C-48497A, para 4.5.3.1Humidity: The coated optical surface will show no signs of deterioration after a 24 hour humidity expo.. |
|||
Thickness | 2000 microns | 78.7 mil | |
American Computer Optics Water White Filter 2 mm Single-Sided Maximum Size: 75" X 110"Abrasion: MIL-C-675C, section 4.5.11Adhesion: MIL-C-48497A, para 4.5.3.1Humidity: The coated optical surface will show no signs of deterioration after a 24 hour humidity exp.. |
|||
Thickness | 2000 microns | 78.7 mil | |
American Computer Optics UV Protection Glass 2 mm Maximum Size: 24" X 36"Abrasion: MIL-C-675C, section 4.5.11Adhesion: MIL-C-48497A, para 4.5.3.1Humidity: The coated optical surface will show no signs of deterioration after a 24 hour humidity expo.. |
|||
Thickness | 2000 microns | 78.7 mil | |
Mo-Sci Corporation GA-80-N Green Filter Glass Applications: Lead-free NVIS green filter glass for Nichia White LED sources.Information provided by Mo-Sci Corporation. |
|||
Thickness | 2000 microns | 78.7 mil | |
SMAC SMACWRAP® EX Damping Material, 0.20 mm SMACWRAP® concept is a smart and lightweight solution to embed into composite structures a very thin viscoelastic material. The SMACWRAP® will then bring damping to the composite structure without.. |