Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 203 microns | 8.00 mil | |
Honeywell ACLAR® 11A (8.00 mil) CTFE Homopolymer, Barrier Film
(discontinued **) Description: ACLAR® 11A is a CTFE homopolymer, high performance barrier film for industrial and electronics applications.Information provided by Honeywell. |
|||
Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
Arlon A3020-R008-16.5 0.020" (0.508 mm) Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate
&nb 2 inches width and 50 inches long. Design/Construction: Side 1: Cured Fusible Silicone Rubber Substrate: 25% sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester Film Th.. |
|||
Thickness | 203 microns | 8.00 mil | Prime Coated 1523 Fiberglass, Substrate |
Arlon 28601M015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Tan gum on glass fiber fabricThis data represents typical values for the production material. The data .. |
|||
Thickness | 203 - 254 microns | 8.00 - 10.0 mil | Overall |
Arlon 48571R009 0.009" (0.229 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specif.. |
|||
Thickness | 203 microns | 8.00 mil | Substrate |
Arlon 51422R020 0.020" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Prime Coated 7628 FiberglassInterleave: 3 mil PolyethyleneThis data represents typical values for the production material and should no.. |
|||
Thickness | 203 microns | 8.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 51576R024A 0.024" (0.610 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat.. |
|||
Thickness | 203 microns | 8.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 51576R024A 0.024" (0.610 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber This data represents typical values for the production mat.. |
|||
Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 51586R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Red silicone gum and rubber on fiberglass clot.. |
|||
Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 51866R020 0.020" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 51986R015 0.0165" (0.419 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flexible heater substrateAppearance: Red colo.. |
|||
Thickness | 203 microns | 8.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55148R036 0.036" (0.914 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2, Layer 2: Uncured Silicone Rubber Side 2, Layer 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber This data r.. |
|||
Thickness | 203 microns | 8.00 mil | Prime Coated 7628 Fiberglass, Substrate |
Arlon P29609R015 0.015" (0.381 mm) Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Layer-on-Layer Product Use: Traction motor insulation, electrical insulationAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the pr.. |
|||
Thickness | >= 203 microns | >= 8.00 mil | Prime Coated 7628 Fiberglass, Substrate |
Arlon R35061R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 203 microns | 8.00 mil | Prime Coated 7628 Fiberglass, Substrate |
Arlon R35066R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
Arlon R35948R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberThis data re.. |
|||
Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
Arlon R39091R036 0.036" (0.914 mm) Uncured Silicone Rubber with Nomex Fabric Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1574 Nomex FabricSide 2: Uncured SiliconeInterleave: Polyethylene This data represents typical values fo.. |
|||
Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-012 |
Arlon T3020-B004 0.020" Self-Fusing, Cured Silicone Rubber Tape with Fiberglass Substrate 1.0 inch wide, 20 mil thick, black, rectangular cross-section, self-fusing silicone tape.Design/Construction:Side 1: Cured Silicone RubberSubstrate: 25% Sinusoidal FiberglassSide 2: Cured Silicone.. |
|||
Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-012 |
Arlon T3030-R004 0.030" (0.762 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate Design/Construction: Side 1: Cured Fusible Silicone RubberSubstrate: 25% Sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester FilmArlon MOX-Tape® Fiberglass Reinforced T.. |
|||
Thickness | 203 microns | 8.00 mil | FEP, Interleave |
Arlon Thermabond®-II 99760N008 0.008" (0.203 mm) Unsupported/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Unsupported/Uncured RubberAppearance: White/gray gumAppearance: White/grey gumThis data Represents typical values for the production material. The data should not be used.. |
|||
Thickness | 203 - 241 microns | 8.00 - 9.50 mil | Overall |
Arlon 44571B008 0.0085" (0.216 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 51231R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical .. |
|||
Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 51271R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneProduct Use: Flexible heater in.. |
|||
Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 51271R037 0.037" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the produ.. |
|||
Thickness | 203 microns | 8.00 mil | Prime Coated 7628 Fiberglass, Substrate |
Arlon 51576X015A 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 51583R018 0.018" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: 2.5 mil LDPESide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave 2: 2.5 mil LDPEThis data represents typical val.. |
|||
Thickness | 203 microns | 8.00 mil | Prime Coated 7628 Fiberglass, Substrate |
Arlon 51976R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production mat.. |
|||
Thickness | 203 microns | 8.00 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55272R024 0.024" (0.610 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. The data should not be use.. |
|||
Thickness | 203 microns | 8.00 mil | Prime Coated 7628 Fiberglass, Substrate |
Arlon R31861R018 0.018" (0.457 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place.. |
|||
Thickness | 203 microns | 8.00 mil | Prime Coated 7628 Fiberglass, Substrate |
Arlon R33991R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 203 microns | 8.00 mil | Substrate; Arlon SQA-TMS-003 |
Arlon R36613N022 0.022" (0.559 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone Rubber Substrate: Style 7628 Heat Cleaned FiberglassSide 2: Cured Silicone RubberSide 2 Interleave: PolyethyleneFiberglas Weave: PlainThis data represents.. |