Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 230 microns
9.06 mil
Isoflon Tisoflon® 10 AD Polytetrafluoroethylene Coated Glass Fabric
PTFE coated glass fabric one side adhesive TISOFLON® - Standard gradeInformation provided by Isoflon.
Thickness 230 microns
9.06 mil
Isoflon Tisoflon® 10G Polytetrafluoroethylene & Graphite Coated Glass Fabric
PTFE + Graphite coated glass fabric TISOFLON® - Black anti-staticInformation provided by Isoflon.
Thickness 230 microns
9.06 mil
Nominal
AK Steel TRAN-COR® H-0 CARLITE® Grain Oriented Electrical Steel
TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l..
Thickness 230 microns
9.06 mil
Nominal
AK Steel TRAN-COR® H-0 CARLITE® DR® Grain Oriented Electrical Steel
TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l..
Thickness 230 microns
9.06 mil
3M Nextel™ AF-11 w/o sizing Aerospace Woven Fabric 312
Information provided by 3M