Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 267 microns | 10.5 mil | |
Hexcel® HexForce™ SGP203-CS Carbon Fabric Hexcel's carbon fibers contain high strength-to-weight and stiffness-to-weight ratios. Carbon fabrics are thermally and electrically conductive and exhibit excellent fatigue resistance. When proper.. |
|||
Thickness | 267 microns | 10.5 mil | Typical; ASTM D374 |
DuPont™ Nomex® 414 Paper, 10 mil Nominal Thickness Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand.. |
|||
Thickness | 267 microns | 10.5 mil | Overall Thickness |
Arlon 49581R010 0.0105" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 1681 FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the .. |
|||
Thickness | 267 microns | 10.5 mil | Layer 2; Arlon SQA-TMS-003 |
Arlon 55579R031H 0.0315" (0.800 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: LDPELayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. T.. |
|||
Thickness | 267 microns | 10.5 mil | Overall; Arlon SQA-TMS-003 |
Arlon R35782R010 0.0105" (0.267 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Top Layer of Side 1: Metalized Polymer Film Bottom Layer of Side 1: Cured Silicone RubberSubstrate: Style 138 FiberglassThis data represents typical values for the production mat.. |
|||
Thickness | 267 - 343 microns | 10.5 - 13.5 mil | Overall |
Arlon 47091R012 0.012" (0.305 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data should not be u.. |
|||
Thickness | 267 microns | 10.5 mil | side1/uncured; Arlon SQA-TMS-003 |
Arlon 51228R020 Silicone Rubber/Fiberglass Laminate Interleave: 1.5 mil PE; Side 1, layer 2: uncured silicone rubber; Side 1, layer 1: Cured silicone rubber; Substrate: 7628 fiberglass; Side 2: cured silicone rubber |
|||
Thickness | 267 microns | 10.5 mil | Layer 2; Arlon SQA-TMS-003 |
Arlon 55279R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s.. |
|||
Thickness | 267 microns | 10.5 mil | Rubber |
Arlon R31030R025 0.025" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberSubstrate: 0.015" Prime Coated 1564 FiberglassThis data represents typical values for the production material and.. |