Polymer Property : Thickness = 27.0 mil Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 584 - 686 microns
23.0 - 27.0 mil
Overall
Arlon 15880T025 0.025" (0.635 mm) Uncured, Unsupported Silicone Rubber on a Mylar Carrier
Design/Construction:Side 1: Uncatalyzed, Unsupported Silicone Rubber on a Mylar CarrierAppearance: Clear silicone gum on polymer filmThis data represents typical values for the production material. ..
Thickness 584 - 686 microns
23.0 - 27.0 mil
Side 1
Arlon 15880T025 0.025" (0.635 mm) Uncured, Unsupported Silicone Rubber on a Mylar Carrier
Design/Construction:Side 1: Uncatalyzed, Unsupported Silicone Rubber on a Mylar CarrierAppearance: Clear silicone gum on polymer filmThis data represents typical values for the production material. ..
Thickness 584 - 686 microns
23.0 - 27.0 mil
Overall
Arlon 19220R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not be used to w..
Thickness 584 - 686 microns
23.0 - 27.0 mil
Overall
Arlon 19571R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place o..
Thickness 635 - 686 microns
25.0 - 27.0 mil
Overall
Arlon 23234R025 0.025" (0.635 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Semi-Cured Silicone Rubber This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications...
Thickness 584 - 686 microns
23.0 - 27.0 mil
Overall
Arlon 31570R025 0.025" (0.635 mm) Uncured Unsupported Silicone on a HDPE Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The dat..
Thickness 584 - 686 microns
23.0 - 27.0 mil
Side 1
Arlon 31570R025 0.025" (0.635 mm) Uncured Unsupported Silicone on a HDPE Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The dat..
Thickness 660 - 686 microns
26.0 - 27.0 mil
Overall
Arlon 56581R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. T..
Thickness 584 - 686 microns
23.0 - 27.0 mil
Overall
Arlon 30580R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on Release Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Release CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The da..
Thickness 584 - 686 microns
23.0 - 27.0 mil
Side 1
Arlon 30580R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on Release Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Release CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The da..
Thickness 584 - 686 microns
23.0 - 27.0 mil
Overall
Arlon 56224R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info..
Thickness 584 - 686 microns
23.0 - 27.0 mil
Overall
Arlon 30600R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on Release Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Release CarrierProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis da..
Thickness 584 - 686 microns
23.0 - 27.0 mil
Side 1
Arlon 30600R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on Release Carrier
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Release CarrierProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis da..
Thickness 584 - 686 microns
23.0 - 27.0 mil
Overall
Arlon 44570R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Layers Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be use..
Thickness 584 - 686 microns
23.0 - 27.0 mil
Overall
Arlon 31580R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on HDPE Carrier  (discontinued **)&
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data ..
Thickness 584 - 686 microns
23.0 - 27.0 mil
Side 1
Arlon 31580R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on HDPE Carrier  (discontinued **)&
Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data ..