Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 584 microns | 23.0 mil | cured, per ply |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T700 12K BW Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Thickness | 584 microns | 23.0 mil | Nominal |
DuPont™ Nomex® 411 Paper, 23 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |
|||
Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Overall |
Arlon 15880T025 0.025" (0.635 mm) Uncured, Unsupported Silicone Rubber on a Mylar Carrier Design/Construction:Side 1: Uncatalyzed, Unsupported Silicone Rubber on a Mylar CarrierAppearance: Clear silicone gum on polymer filmThis data represents typical values for the production material. .. |
|||
Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Side 1 |
Arlon 15880T025 0.025" (0.635 mm) Uncured, Unsupported Silicone Rubber on a Mylar Carrier Design/Construction:Side 1: Uncatalyzed, Unsupported Silicone Rubber on a Mylar CarrierAppearance: Clear silicone gum on polymer filmThis data represents typical values for the production material. .. |
|||
Thickness | 584 microns | 23.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 18609R023 0.023" (0.584 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: PolyethyleneLayer 1: Cured Silicone RubberLayer 2: Uncured Silicone RubberSubstrate: 11523 Style FiberglassThis data represents typical values for the production mate.. |
|||
Thickness | 584 microns | 23.0 mil | overall; Arlon SQA-TMS-003 |
Arlon 18976XA023 Silicone Rubber/Fiberglass Laminate Side 1:cured silicone rubber; Substrate: 11523 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil Polyethylene |
|||
Thickness | 584 microns | 23.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 18986XA023 0.023" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 11523 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the produ.. |
|||
Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Overall |
Arlon 19220R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not be used to w.. |
|||
Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Overall |
Arlon 19571R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Overall |
Arlon 31570R025 0.025" (0.635 mm) Uncured Unsupported Silicone on a HDPE Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The dat.. |
|||
Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Side 1 |
Arlon 31570R025 0.025" (0.635 mm) Uncured Unsupported Silicone on a HDPE Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The dat.. |
|||
Thickness | 584 microns | 23.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55591R062 0.062" (1.57 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene Product Use: Electrical insula.. |
|||
Thickness | 584 microns | 23.0 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 55591R062 0.062" (1.57 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene Product Use: Electrical insula.. |
|||
Thickness | 584 microns | 23.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55833R062 Mar Resistant Press Pad; 1.6 mm Cured Silicone Rubber with Fiberglass Substrate Mar Resistant Press Pad - Product is sold with two finishes options: 55833R062AC - "C-finish" and 55833R062DST - "Smooth with Talc"Design/Construction:Interleave: 3 mil PESide 1: Cured Silicone Ru.. |
|||
Thickness | 584 microns | 23.0 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 55833R062 Mar Resistant Press Pad; 1.6 mm Cured Silicone Rubber with Fiberglass Substrate Mar Resistant Press Pad - Product is sold with two finishes options: 55833R062AC - "C-finish" and 55833R062DST - "Smooth with Talc"Design/Construction:Interleave: 3 mil PESide 1: Cured Silicone Ru.. |
|||
Thickness | >= 584 microns | >= 23.0 mil | Side 2 |
Arlon 56596R045 0.045" (1.14 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silicone gum and rubber on fiberglass with polymer release lin.. |
|||
Thickness | >= 584 microns | >= 23.0 mil | Side 1 |
Arlon R35121R063 0.063" (1.60 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material speci.. |
|||
Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Overall |
Arlon 30580R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on Release Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Release CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The da.. |
|||
Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Side 1 |
Arlon 30580R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on Release Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Release CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The da.. |
|||
Thickness | 584 - 660 microns | 23.0 - 26.0 mil | Overall |
Arlon 56096R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Overall |
Arlon 56224R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info.. |
|||
Thickness | >= 584 microns | >= 23.0 mil | Side 2 |
Arlon R31246R063 0.063" (1.60 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Rubber LayerSide 2: Uncured Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, mate.. |
|||
Thickness | >= 584 microns | >= 23.0 mil | Side 2 |
Arlon R34256R063 0.063" ((1.60 mm) Uncured/Cured Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Rubber LayerSide 2: Uncured Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, mate.. |
|||
Thickness | 584 microns | 23.0 mil | |
3M Safety-Walk™ 280 White Slip-Resistant Fine Resilient Tapes and Treads A fine-textured, slip-resistant surface with a pressure-sensitive adhesive backing provides enhanced safety and comfort in light- and barefoot- traffic areas. For wet, barefoot-traffic areasNon-mine.. |
|||
Thickness | 584 microns | 23.0 mil | |
3M Safety-Walk™ 7705 White Slip-Resistant Fine Resilient Tapes and Treads A fine-textured, slip-resistant surface with a pressure-sensitive adhesive backing provides enhanced safety and comfort in light- and barefoot- traffic areas. For wet, barefoot-traffic areasNon-mine.. |
|||
Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Overall |
Arlon 30600R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on Release Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Release CarrierProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis da.. |
|||
Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Side 1 |
Arlon 30600R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on Release Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on Release CarrierProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis da.. |
|||
Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Overall |
Arlon 44570R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Layers Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be use.. |
|||
Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Overall |
Arlon 31580R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on HDPE Carrier
(discontinued **)& Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data .. |
|||
Thickness | 584 - 686 microns | 23.0 - 27.0 mil | Side 1 |
Arlon 31580R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on HDPE Carrier
(discontinued **)& Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data .. |