Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 305 microns | 12.0 mil | |
Rogers Corporation Poron® 4701-50 Supported Urethane Foam, Firm, PET Supported Firm material used for managing high energy impact with gasketing needs. Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce.. |
|||
Thickness | 305 microns | 12.0 mil | cured laminate, per ply |
Park Electrochemical Nelcote® F-502 Phenolic Prepreg, 581 Quartz Reinforced Nelcote® F-502 is a MIL-R-9299 phenolic resin system suitable for impregnation on any MIL-C-9084 fabric with a compatible finish. F-502 is used in the manufacture of ablative reinforcements in rock.. |
|||
Thickness | 305 microns | 12.0 mil | |
Fibre Glast 530 Plain Weave Carbon Fiber Fabric Graphite fibers contain up to 95% carbon and yield the highest tensile strength in the FRP industry. These fibers woven together form graphite fabric. These fabrics offer higher strength and stiffne.. |
|||
Thickness | 305 microns | 12.0 mil | |
Hexcel® HexForce™ 328 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Thickness | 305 microns | 12.0 mil | |
Hexcel® HexForce™ 1188 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 305 microns | 12.0 mil | at 0.06 MPa |
Zircar Ceramics APA-3 Alumina Paper ZIRCAR Alumina Papers are uniform structures made principally of alumina fiber. APA-3 is a thin uniformly rigidized sheet of alumina fiber and binder. Applications include thermal insulation in lo.. |
|||
Thickness | 305 microns | 12.0 mil | Nominal |
DuPont™ Nomex® 414 Paper, 12 mil Nominal Thickness Nomex® Type 414 is designed for uses requiring a strong, yet flexible and conformable sheet. It is electrically and thermally similar to Type 410. Type 414 was designed as slot insulation in hand.. |
|||
Thickness | 305 microns | 12.0 mil | Nominal |
DuPont™ Nomex® E56 Paper, 12 mil Nominal Thickness Nomex® Type E56 is designed for cost critical uses which require lesser amounts of mechanical and electrical strength than other Nomex® grades. It is thermally similar to Nomex® Type 410 but as.. |
|||
Thickness | 305 microns | 12.0 mil | Backing; ASTM D3652 |
3M 436/Silver Damping Foils Low temperature vibration dampingInformation provided by 3M |
|||
Thickness | 305 microns | 12.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 49481R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1681 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical .. |
|||
Thickness | 305 microns | 12.0 mil | Side 2 |
Arlon 51393R031 0.031 (0.635 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber Pad Life: 150 Cycles (temperature and time dependent)This data represents typical values for the production material. T.. |
|||
Thickness | >= 305 microns | >= 12.0 mil | Side 1 |
Arlon 51582R020 0.020" (0.508 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Inform.. |
|||
Thickness | 305 microns | 12.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55572GA028 0.028" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production material and should not be used as material .. |
|||
Thickness | 305 microns | 12.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55572R030 0.030" (0.762 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Appearance: Red silicone rubber on fiberglass clothThis data Represents typical values for the production material. T.. |
|||
Thickness | 305 microns | 12.0 mil | Layer 2; Arlon SQA-TMS-003 |
Arlon 55589R032 0.034" (0.864 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 FiberglassAppearance: Red silicone gum and rubber on fiberglass This.. |
|||
Thickness | 305 microns | 12.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55590R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. The data should not be us.. |
|||
Thickness | 305 microns | 12.0 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 55638R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater SubstrateAppearance: Red silic.. |
|||
Thickness | 305 microns | 12.0 mil | Prime Coated 1581 Fiberglass, Substrate |
Arlon 57226R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 305 microns | 12.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon Thermabond® 51A42X012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628.. |
|||
Thickness | 305 microns | 12.0 mil | Side 1 |
Arlon 51344R020 0.020" (0.508 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Semi-Cured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to.. |
|||
Thickness | 305 microns | 12.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55272R028 0.028" (0.711 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 162 FiberglassThis data represents typical values for the production material. The data should not be use.. |
|||
Thickness | 305 microns | 12.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55560R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for.. |
|||
Thickness | 305 microns | 12.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 912-10X##-P0 0.012" (0.305 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 12 mil thick, Gray, Rectangular cross-section, Self-fus.. |
|||
Thickness | 305 microns | 12.0 mil | Silicone; Arlon SQA-TMS-003 |
Arlon 91B32R016AC Aluminum Clad Silicone Press Pad with "C-finish" Design/Construction:Side 2: Alloy 1100 H18 Aluminum FoilSide 1: Cured Silicone RubberThis data represents typical values for the production material and should not be used as material specificatio.. |
|||
Thickness | 305 microns | 12.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R38041X012 0.012" (0.305 mm) Uncured Fluorosilicone with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 2116 FiberglassSide 2: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Gray silicone gum.. |
|||
Thickness | 305 microns | 12.0 mil | Nominal |
AK Steel CARLITE® M-5 Grain Oriented Electrical Steel Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce.. |
|||
Thickness | 305 microns | 12.0 mil | ASTM D3652 |
3M Scotch® 393 General Purpose Cloth Tape Scotch® General Purpose Cloth Tape 393 is a polyethylene coated cloth backing coated with a rubber adhesive for moisture-proofing, duct sealing and general purpose applications.Information provided.. |
|||
Thickness | 305 - 356 microns | 12.0 - 14.0 mil | Overall |
Arlon 44686W013 0.013" (0.330 mm) Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber UL Recognition: 220°C per UL Card E54153Appearance: White silicone gum on fiberglassThis data represents typical val.. |
|||
Thickness | 305 microns | 12.0 mil | Rubber; Arlon SQA-TMS-012 |
Arlon T1012-R004-xx 0.012" Self-Fusing Silicone Rubber Tape 1 inch wide, 12 mil thick, red, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.Desi.. |