Physical Properties Metric English Comments
Thickness 790 microns
31.1 mil
Standard
GrafTech GRAFOIL® UCAR®-323 Reinforced PTFE Gasketing
GRAFOIL® Grade UCAR®-323 is a laminated gasket material consisting of multiple plies of woven fiberglass coated with PTFE. It will not support combustion or bacteria. Its applications include:..
Thickness 790 microns
31.1 mil
Overall; Arlon SQA-TMS-003
Arlon 51073R031 0.0311" (0.79 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone Rubber This data represents typical values for the production materi..
Thickness 790 microns
31.1 mil
Overall Thickness; Arlon SQA-TMS-003
Arlon UltraPad™ 51073G031D Silicone-Based Press Pad
Green UltraPad™ D65: Silicone Based Press PadDesign/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberThis data..
Thickness 790 microns
31.1 mil
Overall Thickness; Arlon SQA-TMS-003
Arlon UltraPad™ 51073R031D Silicone-Based Press Pad
UltraPad™ D65: Silicone Based Press PadDesign/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberThis data repre..
Thickness 790 microns
31.1 mil
Overall Thickness; Arlon SQA-TMS-003
Arlon UltraPad™ 55073R031 Silicone-Based Press Pad
UltraPad™ D65: Silicone Based Press PadDesign/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberThis data repre..