Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 3560 microns | 140 mil | Wet |
3M Scotchkote™ GP 120 Epoxy Primer Scotchkote Epoxy Primer GP 120 has been specifically developed as an anti corrosive coating for steel structures that cannot be abrasive blast cleaned.Product Features:Suitable for use on mechanical.. |