Physical Properties Metric English Comments
Thickness 112 microns
4.40 mil
Total
Parker Chomerics CHO-FOIL CCD Shielding Tape
Conductive Adhesive Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or ti..
Thickness 112 microns
4.40 mil
ASTM D3652
3M 201+ General Use Masking Tape
3M™ General Use Masking Tape 201+ is a tan colored crepe paper masking tape for holding, bundling, sealing, non-critical masking applications and a vast number of other jobs where a pressure sensit..
Thickness 112 microns
4.40 mil
Total; ASTM D3652
3M 3367 General Purpose Aluminum Foil Tape
66 lb moisture stable liner. Good for die-cut applications.Information provided by 3M
Thickness 112 microns
4.40 mil
Caliper
3M 9496LE High Strength Double Coated Tape with Adhesives 300LSE and 200MP
3M™ Double Coated Tape 9496LE with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and..
Thickness 112 microns
4.40 mil
ASTM D3652
3M 200 Paper Tape
3M™ Paper Tape 200 is a utility purpose paper tape for holding, bundling, sealing, non-critical masking and a vast number of other jobs where a pressure-sensitive tape is needed.Information provide..