3M 201+ General Use Masking Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M 201+ General Use Masking Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ General Use Masking Tape 201+ is a tan colored crepe paper masking tape for holding, bundling, sealing, non-critical masking applications and a vast number of other jobs where a pressure sensitive tape is needed.Information provided by 3M
Physical Properties Metric English Comments
Thickness 112 microns
4.40 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.3 MPa
4390 psi
ASTM D3756
Elongation at Break 8.0 %
8.0 %
ASTM D3756
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.0 °C
199 °F
for 30 mins
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Natural