Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 114 - 165 microns | 4.50 - 6.50 mil | Overall |
Arlon 48571R005 0.0055" (0.140 mm) Uncured Silicone Rubber with Fiberglass Substrate
(discontinued **)&l Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specif.. |
|||
Thickness | 114 microns | 4.50 mil | Total; ASTM D3652 |
3M 3382 HVAC Construction Foil/PET laminate. Tear resistance. Roof and gutter repair tape.Information provided by 3M |
|||
Thickness | 114 microns | 4.50 mil | Side 1 |
Arlon 56581R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. T.. |
|||
Thickness | >= 114 microns | >= 4.50 mil | Side 2 |
Arlon 56581R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. T.. |
|||
Thickness | 114 - 127 microns | 4.50 - 5.00 mil | with adhesive |
3M Controltac™ 160 Graphic Film 4-mil, opaque white, opaque black and translucent white vinyl film with a matte finish; Pressure-activated adhesives for easy sliding, tacking, snap up and repositioning; Film series 160C-10 also ha.. |
|||
Thickness | 114 - 127 microns | 4.50 - 5.00 mil | with adhesive |
3M Controltac™ 8640C ES Graphic Film with Comply™ Adhesive This 4-mil film offers great versatility along with slidable, repositionable, pressure activated adhesive. This long term durable and removable film has excellent hiding power and stability, making .. |
|||
Thickness | 114 microns | 4.50 mil | Paper liner |
3M Cushion-Mount™ 1920S Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Thickness | 114 microns | 4.50 mil | Paper liner |
3M Cushion-Mount™ E1020 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 114 microns | 4.50 mil | Paper liner |
3M Cushion-Mount™ E1215 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 114 microns | 4.50 mil | Paper liner |
3M Cushion-Mount™ E1520 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 114 microns | 4.50 mil | Film Liner |
3M Cushion-Mount™ E1840 Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |
|||
Thickness | 114 microns | 4.50 mil | Film Liner |
3M Cushion-Mount™ E1860H Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |
|||
Thickness | 114 microns | 4.50 mil | Paper liner |
3M Cushion-Mount™ E1915S Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 114 - 127 microns | 4.50 - 5.00 mil | with adhesive |
3M Scotchcal™ 3470 Graphic Film 4-mil, opaque white and opaque black, vinyl film with a matte finish; Pressure-sensitive adhesive; Excellent hiding power; Removable with heatInformation provided by 3M |
|||
Thickness | 114 - 127 microns | 4.50 - 5.00 mil | with adhesive |
3M Scotchcal™ IJ355%-10 Changeable Graphic Film 4-mil, opaque white vinyl film with a matte finish; Excellent hiding power; Pressure-sensitive adhesive; Changeable for clean removable without heat or chemicalsInformation provided by 3M |
|||
Thickness | 114 microns | 4.50 mil | wet |
3M Scotchkote™ FB856 Urethane Primer Scotchkote Urethane Primer FB 856 has been specifically developed as a primer/sealer for porous mineral, timber and asphalt surfaces used on floors and roofs.Product Features:Combines good applicati.. |
|||
Thickness | 114 microns | 4.50 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 49100R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1681 FiberglassProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass fabricTh.. |
|||
Thickness | 114 - 127 microns | 4.50 - 5.00 mil | with adhesive |
3M Controltac™ 162-10 Graphic Film 4-mil, opaque white, or clear vinyl film; Slideable and repositionable; Excellent hiding power (white film); Easily removable and Outstanding resistance to dirt and other environmental factors and w.. |
|||
Thickness | 114 - 127 microns | 4.50 - 5.00 mil | with adhesive |
3M Controltac™ 162-114 Graphic Film 4-mil, opaque white, or clear vinyl film; Slideable and repositionable; Excellent hiding power (white film); Easily removable and Outstanding resistance to dirt and other environmental factors and w.. |
|||
Thickness | 114 - 127 microns | 4.50 - 5.00 mil | with adhesive |
3M Controltac™ 3500C Changeable Graphic Film with Comply™ Adhesive 4-mil, opaque white vinyl film with a matte finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Air release channels for fast, easy, bub.. |
|||
Thickness | 114 microns | 4.50 mil | Paper liner |
3M Cushion-Mount™ 1015M Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Thickness | 114 microns | 4.50 mil | Paper liner |
3M Cushion-Mount™ 1020 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Thickness | 114 microns | 4.50 mil | Paper liner |
3M Cushion-Mount™ 1020M Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Thickness | 114 microns | 4.50 mil | Paper liner |
3M Cushion-Mount™ 1115 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Thickness | 114 microns | 4.50 mil | ASTM D3652 |
3M 4F94 Fire Retardant Carpet Protective Tape 3M™ Fire Retardant Carpet Protective Tape 4F94 is a flame retardant, thicker polyethylene tape with a very high-tack adhesive system used for temporary protection of carpets during construction or .. |
|||
Thickness | 114 microns | 4.50 mil | Paper liner |
3M Cushion-Mount™ E1320 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 114 microns | 4.50 mil | Paper liner |
3M Cushion-Mount™ E1720 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 114 - 127 microns | 4.50 - 5.00 mil | with adhesive |
3M Scotchcal™ 3475 Graphic Film 4-mil, opaque white and opaque black, vinyl film with a matte finish; Pressure-sensitive adhesive; Excellent hiding power; Removable with heatInformation provided by 3M |
|||
Thickness | >= 114 microns | >= 4.50 mil | Side 1, Uncured |
Arlon 44568R016 0.016" (0.406 mm) Cured/Uncured Layers Uncured Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, mat.. |
|||
Thickness | 114 microns | 4.50 mil | |
Hexcel® HexForce™ 1579 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |