Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 432 - 508 microns | 17.0 - 20.0 mil | Range of Thicknesses Available |
Rogers Corporation Poron® 4701-50 Thin as Cast Urethane Foam, Firm, Thin as Cast Firm material used for managing high energy impact with gasketing needs. Standard available thickness range from 0.012" to 0.500" (0.30 mm to 12.7 mm).Features and Benefits of PORON Products: Exce.. |
|||
Thickness | 432 microns | 17.0 mil | |
Polystrand ThermoPro™ IE7015 Unitape Unidirectional Polypropylene-Glass Composite Fiber Orientation is 0°.Polystrand ThermoPro™ combines continuous E-Glass (ThermoPro-E™) structural reinforcing fibers in either a polyethylene or polypropylene proprietary thermoplastic polymer .. |
|||
Thickness | 432 microns | 17.0 mil | Gauge, nominal |
Mid-Mountain Materials ARMATEX® SF17 Industrial Silicone Rubber Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Thickness | 432 microns | 17.0 mil | Gauge, nominal |
Mid-Mountain Materials ARMATEX® SF17 Silicone Rubber Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Thickness | 432 microns | 17.0 mil | Side 1 |
Arlon 51570R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The data should not be used to wri.. |
|||
Thickness | 432 microns | 17.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 51866R015 0.0170" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Thickness | 432 microns | 17.0 mil | overall; Arlon SQA-TMS-003 |
Arlon 51976XA015 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Thickness | 432 microns | 17.0 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 55146R040 0.040"(1.02 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red sil.. |
|||
Thickness | 432 microns | 17.0 mil | Prime Coated 162 Fiberglass, Substrate |
Arlon 55589W028 0.028" (0.711 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber LayerSide 2: Uncured Silicone Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or.. |
|||
Thickness | 432 microns | 17.0 mil | Prime Coated 1564 Fiberglass, Substrate |
Arlon 56596R045 0.045" (1.14 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silicone gum and rubber on fiberglass with polymer release lin.. |
|||
Thickness | 432 microns | 17.0 mil | Prime Coated 1564 Fiberglass, Substrate |
Arlon 56596R065 0.065" (1.65 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silicone gum and rubber on fiberglass with polymer release li.. |
|||
Thickness | 432 - 584 microns | 17.0 - 23.0 mil | Overall |
Arlon 920-07Rxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularWidth, inches: 0.75Arlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tap.. |
|||
Thickness | 432 - 584 microns | 17.0 - 23.0 mil | Overall |
Arlon LW202Bxx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Thickness | 432 - 584 microns | 17.0 - 23.0 mil | Overall |
Arlon LW202Txx-P0 0.020" (0.508 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction:Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for sub.. |
|||
Thickness | 432 microns | 17.0 mil | Tape |
3M Cushion-Mount™ 1015 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Thickness | 432 - 559 microns | 17.0 - 22.0 mil | Side 1 |
Arlon R30651R062 0.062" (1.57 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 432 - 559 microns | 17.0 - 22.0 mil | Side 2 |
Arlon R30651R062 0.062" (1.57 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 432 microns | 17.0 mil | Tape |
3M Cushion-Mount™ E1115 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 432 microns | 17.0 mil | Tape |
3M Cushion-Mount™ E1315 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 432 microns | 17.0 mil | Tape |
3M Cushion-Mount™ E1515 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 432 microns | 17.0 mil | Tape |
3M Cushion-Mount™ E1715 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Thickness | 432 microns | 17.0 mil | substrate; Arlon SQA-TMS-003 |
Arlon R36319R028 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: Cured silicone rubber; Substrate: 162 fiberglass |
|||
Thickness | 432 microns | 17.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R37208T017 0.017" (0.432 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Liner Design/Construction: Liner: PTFE Coated Fiberglass Side 1: Uncured Silicone Rubber Substrate: Laminated Tefzel® Substrate: Treated for adhesionThis data represents typical values for the productio.. |
|||
Thickness | 432 microns | 17.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R38026B017 0.017" (0.432 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1165 FiberglassSide 2: Uncured Silicone Rubber Interleave: LDPEThis data represents typical values for the production material. The.. |
|||
Thickness | 432 microns | 17.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 51344R025 0.025" (0.635 mm) Semi-Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Semi-Cured Silicone RubberSubstrate: Style 7628 FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values fo.. |
|||
Thickness | 432 microns | 17.0 mil | Tape; ASTM D3652 |
3M 9343 Conformable Sound Management Film 3M™ Conformable Sound Management Film 9343 is designed for the reduction of noise, vibration, squeaks, and rattles in automotive interior applications. The currently available materials for these a.. |
|||
Thickness | 432 microns | 17.0 mil | Tape |
3M Cushion-Mount™ 1115 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Thickness | 432 microns | 17.0 mil | Tape |
3M Cushion-Mount™ 1915M Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Thickness | 432 microns | 17.0 mil | Tape |
3M Cushion-Mount™ E1920 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |