Physical Properties Metric English Comments
Thickness 1370 - 1680 microns
54.0 - 66.0 mil
Overall
Arlon 10502N060 0.060" (1.52 mm) Cured/Post-Cured Unsupported Silicone Rubber
Design/Construction:Side 1: Cured/Post-Cured Unsupported Silicone Rubber Appearance: Red silicone rubberThis data represents typical values for the production material. The data should not be used t..
Thickness 1370 - 1680 microns
54.0 - 66.0 mil
Side 1
Arlon 10502N060 0.060" (1.52 mm) Cured/Post-Cured Unsupported Silicone Rubber
Design/Construction:Side 1: Cured/Post-Cured Unsupported Silicone Rubber Appearance: Red silicone rubberThis data represents typical values for the production material. The data should not be used t..
Thickness 1370 - 1680 microns
54.0 - 66.0 mil
Overall
Arlon 10842S060 0.060" (1.52 mm) Fully Cured, Unsupported, Silicone Rubber
Design/Construction:Side 1: Fully Cured, Unsupported, Silicone Rubber Appearance: Dark red silicone rubberThis data represents typical values for the production material. The data should not be used..
Thickness 1370 - 1680 microns
54.0 - 66.0 mil
Side 1
Arlon 10842S060 0.060" (1.52 mm) Fully Cured, Unsupported, Silicone Rubber
Design/Construction:Side 1: Fully Cured, Unsupported, Silicone Rubber Appearance: Dark red silicone rubberThis data represents typical values for the production material. The data should not be used..
Thickness 1370 - 1680 microns
54.0 - 66.0 mil
Overall
Arlon R31246R060 0.060" (1.52 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Rubber LayerSide 2: Uncured Rubber Layer This data Represents typical values for the production material. The data should not be used to write, or in place of, mate..