Material Notes:
Design/Construction:Side 1: Cured/Post-Cured Unsupported Silicone Rubber Appearance: Red silicone rubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Thickness 76.2 microns
3.00 mil
Polyethylene Interleave
1370 - 1680 microns
54.0 - 66.0 mil
Overall
1370 - 1680 microns
54.0 - 66.0 mil
Side 1
Mechanical Properties Metric English Comments
Hardness, Shore A 50 - 60
50 - 60
Compound Property
Tensile Strength 7.45 - 9.10 MPa
1080 - 1320 psi
Compound Property
Elongation at Break 540 - 660 %
540 - 660 %
Compound Property
100% Modulus >= 0.00172 GPa
>= 0.250 ksi
Compound Property
Tear Strength >= 43.8 kN/m
>= 250 pli
Compound Property
Compression Set <= 28 %
<= 28 %
After Post Cure, Compound Property
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength >= 15.7 kV/mm
>= 400 kV/in
Compound Property
Descriptive Properties Value Comments
Color Translucent
Total Product Weight (oz/yd2) 62.1 - 75.9
Users viewing this material also viewed the following: