Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 737 - 889 microns | 29.0 - 35.0 mil | Side 1 |
Arlon 75400R045 0.045" (1.14 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Info.. |