Physical Properties Metric English Comments
Vapor Pressure 0.000387 bar

@Temperature 20.0 °C
0.290 torr

@Temperature 68.0 °F
LyondellBasell NMP N-methyl-2-pyrrolidone
Available in electronic grade.Information provided by Lyondell.