Physical Properties | Metric | English | Comments |
---|---|---|---|
Vapor Pressure | 0.000387 bar @Temperature 20.0 °C |
0.290 torr @Temperature 68.0 °F |
|
LyondellBasell NMP N-methyl-2-pyrrolidone Available in electronic grade.Information provided by Lyondell. |